Saru Silver
Grade of
Brazing Alloy |
Nominal
Composition % |
Melting
Range |
International
Standards |

Technical
Details |

MSDS |

Ag |

Cu |

Zn |

Cd |

Others |

°C |

DIN:8513 |

AWS:A5.8 |

SILVER 50N |

50 |

15.5 |

15.5 |

16 |

3Ni |

645-690 |

L-Ag50CdNi |

BAg-3 |

To be provided |

 |
| Is a
general purpose alloy with excellent mechanical properties. The
nickel improves wetting on carbides and produces a less free flowing
alloy. This gives a thicker braze joint, better able to accommodate
higher stresses. |

SILVER 49 (MnNi) |

49 |

16 |

23 |

- |

7.5Mn, 4.5Ni |

680-700 |

L-Ag49 |

BAg-22 |

To be provided |

 |
| Is a
general purpose alloy with excellent mechanical properties. The
nickel improves wetting on carbides and produces a less free flowing
alloy. This gives a thicker braze joint, better able to accommodate
higher stresses. |

SILVER 49A(MnNi) |

49 |

27.5 |

20.5 |

- |

2.5Mn, 0.5Ni |

670-690 |

- |

- |

To be provided |

 |
| For
brazing tungsten carbides and substances which are difficult to wet. |

SILVER 40N |

40 |

30 |

28 |

- |

2Ni |

671-775 |

- |

BAg-4 |

To be provided |

 |
| Is
economical alloys with good wetting characteristics. Used
extensively for carbide tip brazing, but its application is
restricted by its relatively high melting points. |

SILVER 405N |

40 |

30 |

25 |

- |

5Ni |

660-860 |

- |

- |

To be provided |

 |
| For
tungsten carbide and stainless steels. |

SILVER 27 |

27 |

38 |

20 |

- |

9.5Mn, 5.5Ni |

680-830 |

L-Ag27 |

BAg-4 |

To be provided |

 |
| Is
economical alloys with good wetting characteristics, used
preferrably for brazing hard metals to steel mountings. Addition of
Nickel and Manganese improves wettability on tungsten and molybdenum
materials.. Its application is restricted by its relatively high
melting points. |
|
|